Bend test – Qualicoat Testing

All organic coatings except class 2 and 3 powder coatings: EN ISO 1519 Class 2 and 3 powder coatings: EN ISO 1519 followed by a tape pull adhesion test as specified below: Apply an adhesive tape to the significant surface of the test panel following the mechanical deformation. Cover the area by pressing down firmly against the coating to eliminate voids or air pockets. Pull the tape off sharply at right angles to the plane of the panel after 1Read More …

Resistance to boiling water- Qualicoat Testing

Method 1 with boiling water: 2 hours immersion in boiling demineralised water (maximum 10 μS at 20°C). Remove the test sample and allow it to cool down to room temperature. Apply an adhesive tape (see § 2.4) to the surface, ensuring that no air is trapped. After one minute, remove the tape at an angle of 45° with a sharp even pull. Method 2 with a pressure cooker: (to be used for powder and electrophoretic coatings only) Add demineralised waterRead More …

Antique Red Gold/ YK-EPR378

Antique Red Gold Powder Paint Colors Code:YK-EPR378 Color: Red background with gold vein Chemistry System: Epoxy Polyester Gloss: High gloss Surface: Antique wrinkle vein Use : For indoor Application: Sprayed with electrostatic gun Coat layer: One coat layer SEND INQUIRY

Dark Green Hammer/ YK-EP8GH-H17

Dark Green Hammer Powder Paint Color Code:YK-EP8GH-H17 Color: Dark green,similar to RAL6005 Chemistry System: Epoxy Polyester Gloss: High gloss Surface: Hammer wrinkle vein Use : For indoor Application: Sprayed with electrostatic gun Coat layer: One coat layer SEND INQUIRY

Electrostatic Painting Process

Electrostatic painting is a process in which a spray gun tip is electrostatically charged; making the paint charged electrically; thereby allowing the paint to be attracted to a grounded surface. This process wastes almost no paint through normal air flow, wind, or dripping. This is because the paint particles are actually attracted to the surface you are painting like a magnet. However, in order for the process to work the object you are painting has to be grounded. Electrostatic sprayingRead More …

Accelerated weathering test for Qualicoat

EN ISO 11341 Luminous intensity: 550 ± 20 W/m2 (290 – 800 nm) Black standard temperature: 65 ± 5°C Demineralised water: maximum 10 μS Special UV filter (290 nm) Cycles of 18 minutes in a wet medium and 102 minutes in a dry medium. After 1000 hours exposure (2000 hours for class 3), the test panels should be rinsed with demineralised water and checked for: Gloss variation: EN ISO 2813 angle of incidence 60° Colour change: ΔE CIELAB formula according toRead More …

Impact test for Qualicoat

(for powder coatings only) The impact shall be carried out on the reverse side, whereas the results shall be assessed on the coated side. -Class 1 powder coatings (one- and two-coat), energy: 2.5 Nm: EN ISO 6272- 2 (indenter diameter: 15.9 mm) -Two-coat PVDF powder coatings, energy: 1.5 Nm: EN ISO 6272-1 or EN ISO 6272-2 / ASTM D 2794 (indenter diameter: 15.9 mm) -Class 2 and 3 powder coatings, energy: 2.5 Nm: EN ISO 6272-1 or EN ISO 6272-2Read More …